| JOURNAL HOME | HELP | CONTACT PUBLISHER | SUBSCRIBE | ARCHIVE | SEARCH | TABLE OF CONTENTS |
Kent State University, Department of Chemistry, Kent, OH, United States
This study compared surface characteristics and dissolution behavior of well-crystallized (KGa-1b) and poorly crystallized (KGa-2) kaolinite standards. Atomic force microscopy (AFM) revealed that particles of KGa-1b generally have nicely hexagonal micromorphology and crystallographically controlled microtopographic features. Particles of KGa-2 are also hexagonal, but their micromorphology tends to be more rounded. Basal-plane surfaces tend to be more irregular with fewer clearly crystallographically controlled features. KGa-1b particles tend to be larger in diameter and thicker than KGa-2 particles. Micromorphologic measurements showed that both KGa-1b and KGa-2 have modal edge- to total surface-area ratios of approximately 0.1 (mean approximately 0.2), although these measurements did not include the potentially large contribution of basal-plane step edges (additional 20% or more). Dissolution experiments were conducted in oxalic acid and inorganic acids at pH 3, 22 degrees C, I = 0.01 M, under batch dissolution conditions. Dissolution rates (measured as Si release) in 1 mM oxalic acid were approximately twice as fast for KGa-2 as for KGa-1b (2.27 vs. 0.96 nmol/m 2 .h). Rates for KGa-2 and KGa-1b were similar in HNO 3 (0.86 and 1.16 nmol/m 2 .h, respectively). The comparable rates for these two sedimentary kaolinites and for a hydrothermal kaolinite studied by Wieland and Stumm (1992) suggests that the fundamental structure of kaolinite, rather than specific surface details, exerts the greatest influence on dissolution kinetics. High-performance cation exchange chromatography (HP-CEC) was used to determine the distributions of monomeric Al species over the course of kaolinite dissolution. For dissolution in 1 mM oxalate, Al-oxalates were observed almost exclusively in agreement with results of equilibrium speciation calculations. For dissolution in HNO 3 , the peak representing uncomplexed Al species, Al 1 , was predominant but not exclusive, as predicted by calculations. A peak having a retention time characteristic of species with +2 charge may be evidence for an AlOSi(OH) (super 2+) 3 species, and warrant further investigation.
This record provided courtesy of AGI/GeoRef.
This article has been cited by other articles:
![]() |
S. E. Hepinstall, B. F. Turner, and P. A. Maurice EFFECTS OF SIDEROPHORES ON Pb AND Cd ADSORPTION TO KAOLINITE Clays and Clay Minerals, December 1, 2005; 53(6): 557 - 563. [Abstract] [Full Text] [PDF] |
||||
![]() |
F. FRANCO and M. D. RUIZ CRUZ Factors influencing the intercalation degree ('reactivity') of kaolin minerals with potassium acetate, formamide, dimethylsulphoxide and hydrazine Clay Minerals, June 1, 2004; 39(2): 193 - 205. [Abstract] [Full Text] [PDF] |
||||
![]() |
null Hong Hanlie, H. Hong, Z. Sun, Z. Fu, and X. Min ADSORPTION OF AUCL-4 BY KAOLINITES: EFFECT OF pH, TEMPERATURE AND KAOLINITE CRYSTALLINITY Clays and Clay Minerals, October 1, 2003; 51(5): 493 - 501. [Abstract] [Full Text] [PDF] |
||||
![]() |
M. Bentabol, M. BENTABOL, M. D. RUIZ CRUZ, F. J. HUERTAS, and J. LINARES Hydrothermal transformation of kaolinite to illite at 200 and 300{degrees}C Clay Minerals, June 1, 2003; 38(2): 161 - 172. [Abstract] [Full Text] [PDF] |
||||
![]() |
N. U. Yamaguchi, N. U. Yamaguchi, A. C. Scheinost, and D. L. Sparks INFLUENCE OF GIBBSITE SURFACE AREA AND CITRATE ON Ni SORPTION MECHANISMS AT pH 7.5 Clays and Clay Minerals, December 1, 2002; 50(6): 784 - 790. [Abstract] [Full Text] [PDF] |
||||
![]() |
B. R. Bickmore, K. L. Nagy, P. E. Sandlin, and T. S. Crater Quantifying surface areas of clays by atomic force microscopy American Mineralogist, May 1, 2002; 87(5-6): 780 - 783. [Abstract] [Full Text] [PDF] |
||||
![]() |
D. Bosbach, L. Charlet, B. Bickmore, and M. F. Hochella Jr. The dissolution of hectorite: In-situ, real-time observations using atomic force microscopy American Mineralogist, September 1, 2000; 85(9): 1209 - 1216. [Abstract] [Full Text] [PDF] |
||||
![]() |
J. M. Hanchar, K. L. Nagy, P. Fenter, R. J. Finch, D. J. Beno, and N. C. Sturchio Quantification of minor phases in growth kinetics experiments with powder X-ray diffraction American Mineralogist, September 1, 2000; 85(9): 1217 - 1222. [Abstract] [Full Text] [PDF] |
||||
| JOURNAL HOME | HELP | CONTACT PUBLISHER | SUBSCRIBE | ARCHIVE | SEARCH | TABLE OF CONTENTS |